Triethanolamine (TEA)
Formula C6H15NO3 · CAS 102-71-6
Also called Trolamine
What people pick
- Also works
- PVDF (Kynar), EPDM, FFKM
- Avoid
- PVC (rigid), FKM (Viton), Nitrile (Buna-N, NBR)
- If it must be metal
- 316 stainless steel
- Peristaltic tubing
- Santoprene (EPDM/PP TPV)Santoprene rated A; Blue-White rates Flex-A-Prene C, Flex-A-Chem D, Flex-A-Thane D.
- Aflas preferred
- Viscous
- EPDM, not FKM
Why
For TEA a PP or PVDF (Kynar) head is the usual pick, both rated excellent; PVC is only fair. TFE/P (AFLAS) seals are rated excellent and EPDM good, while FKM (Viton) and NBR are rated not recommended. 316 stainless is rated excellent.
From our applications engineers. Every pick is rated A or B by the guides at that strength.
13 of 13 materials
| Material | Strength not stated |
|---|---|
| metal | |
| metal | |
| plastic Usual pick | |
| plastic | |
| plastic | |
| plastic | |
| elastomer Usual pick | |
| plastic | |
| elastomer | |
| plastic | |
| plastic Avoid | |
| elastomer Avoid | |
| plastic |
- Excellent
- Good
- Fair
- Poor
- Estimate
- – No data
Bars: our confidence, 1 to 3. A temperature under the bars is the lowest limit a guide states. Orange dot: use with care; open the rating for why. Grey: an estimate, because no guide rates it. Select any rating for the detail.
Ratings combine published chemical guides, weighted, with Cole-Parmer's printed chart breaking ties. Check the maker and your own conditions before you order. Dataset 2026-11-16-7f6e10a9