Trichloroethylene (TCE)
Formula C2HCl3 · CAS 79-01-6
Also called 1,1,2-Trichloroethene, 1,1-Dichloro-2-Chloroethylene, 1-Chloro-2,2-Dichloroethylene, Acetylene Trichloride, HCC-1120, Trethylene, Triclene
What people pick
- Also works
- PTFE (Teflon), FFKM
- Avoid
- PVC (rigid), Polypropylene, CPVC, EPDM, Nitrile (Buna-N, NBR), Aflas (TFE/P, FEPM)
- Peristaltic tubing
- No pump tube suits it: Flex-A-Prene D, Flex-A-Chem D, Flex-A-Thane D.
- PVDF preferred
- FKM, not EPDM
- Attacks plastics
Why
TCE attacks PVC and PP (D), so the plastic head is PVDF (Kynar). FKM (Viton) is the seal (A, expect some swelling); EPDM, nitrile and TFE/P (AFLAS) fail.
From our applications engineers. Every pick is rated A or B by the guides at that strength.
13 of 13 materials
| Material | Strength not stated |
|---|---|
| metal | |
| metal | |
| plastic | |
| plastic Usual pick | |
| elastomer Usual pick | |
| plastic Avoid | |
| elastomer Avoid | |
| plastic Avoid | |
| plastic | |
| plastic | |
| plastic | |
| plastic Avoid | |
| elastomer Avoid |
- Excellent
- Good
- Fair
- Poor
- – No data
Bars: our confidence, 1 to 3. A temperature under the bars is the lowest limit a guide states. Orange dot: use with care; open the rating for why. Select any rating for the detail.
Ratings combine published chemical guides, weighted, with Cole-Parmer's printed chart breaking ties. Check the maker and your own conditions before you order. Dataset 2026-11-16-7f6e10a9