Sulfamic Acid
Formula H3NSO3 · CAS 5329-14-6
What people pick
- Also works
- Polypropylene, Hypalon (CSPE / CSM)
- Avoid
- FKM (Viton), 316 stainless steel, Alloy 20 (Carpenter 20)
- If it must be metal
- Hastelloy C / Alloy C (grade not stated)
- Peristaltic tubing
- No maker tube rating.
- PVC is the usual head
- EPDM, not FKM
- Avoid 316
Why
Sulfamic acid suits PVC or PP heads, both rated excellent, with EPDM seals; FKM (Viton) is rated fair to poor on one guide and PVDF (Kynar) only good. 316 stainless and Alloy 20 are rated fair to poor; Hastelloy C is rated excellent.
From our applications engineers. Every pick is rated A or B by the guides at that strength.
13 of 13 materials
| Material | Strength not stated |
|---|---|
| plastic | |
| plastic | |
| metal | |
| plastic Usual pick | |
| plastic | |
| elastomer Usual pick | |
| elastomer | |
| plastic | |
| plastic | |
| plastic | |
| plastic | |
| metal Avoid | |
| elastomer Avoid |
- Excellent
- Good
- Fair
- Poor
- Estimate
- – No data
Bars: our confidence, 1 to 3. A temperature under the bars is the lowest limit a guide states. Orange dot: use with care; open the rating for why. Grey: an estimate, because no guide rates it. Select any rating for the detail.
Ratings combine published chemical guides, weighted, with Cole-Parmer's printed chart breaking ties. Check the maker and your own conditions before you order. Dataset 2026-11-16-7f6e10a9