Paraffin

CAS 8002-74-2

What people pick

HeadPVC (rigid) or Polypropylene or PVDF (Kynar)
SealsFKM (Viton)
Also works
Nitrile (Buna-N, NBR)
Avoid
EPDM
Peristaltic tubing
Santoprene rated A (diaphragm-pump guides). No Blue-White/LMI rating; estimate: Flex-A-Thane likely B.
  • FKM, not EPDM
Why

PVC, PP and PVDF (Kynar) heads all rate A, with FKM (Viton) or nitrile seals. EPDM swells in hydrocarbons and rates D. If the paraffin is pumped molten, temperature rather than chemistry limits the plastics.

From our applications engineers. Every pick is rated A or B by the guides at that strength.

13 of 13 materials

MaterialStrength not stated
metal
elastomer
Usual pick
plastic
Usual pick
plastic
plastic
Usual pick
plastic
plastic
Usual pick
plastic
elastomer
metal
plastic
plastic
elastomer
Avoid
  • Excellent
  • Good
  • Fair
  • Poor
  • Estimate
  • – No data

Bars: our confidence, 1 to 3. A temperature under the bars is the lowest limit a guide states. Orange dot: use with care; open the rating for why. Grey: an estimate, because no guide rates it. Select any rating for the detail.

Ratings combine published chemical guides, weighted, with Cole-Parmer's printed chart breaking ties. Check the maker and your own conditions before you order. Dataset 2026-11-16-7f6e10a9