Nitric Acid
Formula HNO3 · CAS 7697-37-2
Also called Acidum nitricum, Aqua fortis, Eau forte, Hydrogen nitrate, Spirit of niter
Sold at 67% (42 °Bé)
What people pick
PVC drops to good (B) at this strength; PVDF is the safer head.
- Also works
- PTFE (Teflon), FFKM
- Avoid
- EPDM, Hypalon (CSPE / CSM), Nitrile (Buna-N, NBR), CPVC, Acrylic (PMMA), Alloy 20 (Carpenter 20)
- If it must be metal
- 316 stainless steel316 is the usual nitric metal: excellent to 60 %, good above; C276 and titanium rate excellent.
- Peristaltic tubing
- Flex-A-Prene is A to 35 % but not for 68-71 %; avoid Flex-A-Thane at any strength.
- PVDF preferred
- Seal choice is critical
- Depends on strength
Why
At commercial strength (60-70 %) the standard pick is a PVDF (Kynar) head with PTFE seals: FKM (Viton) is only fair there and EPDM is not recommended. Below 60 % FKM is rated excellent, and PVC handles dilute acid well. PP is fine dilute but embrittles in stronger acid; 316 stainless is a classic nitric acid metal.
From our applications engineers. Every pick is rated A or B by the guides at that strength.
13 of 13 materials
| Material | 0–10 % | 10–30 % | 30–60 % | 60–100 % |
|---|---|---|---|---|
| plastic | ||||
| metal | ||||
| elastomer Usual pick | ||||
| metal | ||||
| plastic Usual pick | ||||
| plastic Avoid | ||||
| plastic | ||||
| elastomer | ||||
| plastic | – | |||
| plastic | ||||
| plastic | ||||
| plastic Avoid | ||||
| elastomer Avoid |
- Excellent
- Good
- Fair
- Poor
- – No data
Bars: our confidence, 1 to 3. A temperature under the bars is the lowest limit a guide states. Orange dot: use with care; open the rating for why. Select any rating for the detail.