Methylene Diphenyl Diisocyanate (MDI)

Formula C15H10N2O2 · CAS 101-68-8

Also called MDI

Pumping notes
Crystallizes
Freezes near room temperature
Reacts with moisture

What people pick

HeadPTFE (Teflon)
SealsFFKM or PTFE (Teflon)
Also works
Polypropylene, PVDF (Kynar), EPDM
Avoid
FKM (Viton), Nitrile (Buna-N, NBR)
If it must be metal
316 stainless steel316 stainless rates A; keep it dry.
Peristaltic tubing
No maker tube rating.
  • PTFE only
  • Few guides rate it
  • Crystallizes
Why

PTFE is the head rated A, and 316 stainless is a normal material for isocyanates (A). PP and PVDF (Kynar) rate B on estimate-based data. For seals use FFKM or PTFE; FKM (Viton) rates C. The usual problem with MDI is moisture, which forms solids, not attack.

From our applications engineers. Every pick is rated A or B by the guides at that strength.

13 of 13 materials

MaterialStrength not stated
plastic
Usual pick
metal
metal
elastomer
plastic
plastic
plastic
plastic
elastomer
Avoid
elastomer
plastic
plastic
plastic
  • Excellent
  • Good
  • Fair
  • Poor
  • Estimate
  • – No data

Bars: our confidence, 1 to 3. A temperature under the bars is the lowest limit a guide states. Orange dot: use with care; open the rating for why. Grey: an estimate, because no guide rates it. Select any rating for the detail.

Ratings combine published chemical guides, weighted, with Cole-Parmer's printed chart breaking ties. Check the maker and your own conditions before you order. Dataset 2026-11-16-7f6e10a9