Methacrylic Acid
Formula C4H6O2 · CAS 79-41-4
What people pick
- Also works
- PVDF (Kynar), FFKM, EPDM
- Avoid
- FKM (Viton), Hypalon (CSPE / CSM), Nitrile (Buna-N, NBR)
- If it must be metal
- 316 stainless steel
- Peristaltic tubing
- Santoprene (diaphragm-pump guides) rated A. No Blue-White/LMI tube rating; reference only: Norprene rated A.
- Seal choice is critical
- EPDM, not FKM
Why
For methacrylic acid PP and PVDF (Kynar) heads are rated excellent; PVC is likely poor (estimate). Seals are the hard part: FKM (Viton) is only fair, CSPE (Hypalon) and NBR are rated not recommended and EPDM good, so PTFE seals are the safe pick. 316 stainless is rated excellent.
From our applications engineers. Every pick is rated A or B by the guides at that strength.
13 of 13 materials
| Material | Strength not stated |
|---|---|
| plastic Usual pick | |
| metal | |
| metal | |
| plastic Usual pick | |
| plastic | |
| plastic | |
| plastic | |
| elastomer | |
| elastomer | |
| elastomer Avoid | |
| plastic | |
| plastic | |
| plastic |
- Excellent
- Good
- Fair
- Poor
- Estimate
- – No data
Bars: our confidence, 1 to 3. A temperature under the bars is the lowest limit a guide states. Orange dot: use with care; open the rating for why. Grey: an estimate, because no guide rates it. Select any rating for the detail.
Ratings combine published chemical guides, weighted, with Cole-Parmer's printed chart breaking ties. Check the maker and your own conditions before you order. Dataset 2026-11-16-7f6e10a9