Hydrofluoric Acid
Formula HF · CAS 7664-39-3
Also called Fluorhydric acid, Hydrogen fluoride
“Concentrated” usually means 49–49 %.
Sold at 49% · 70%
What people pick
- Also works
- Polypropylene, PTFE (Teflon), Aflas (TFE/P, FEPM)
- Avoid
- EPDM, Nitrile (Buna-N, NBR), Glass-filled polypropylene, CPVC, PEEK, Ceramic (alumina, Al2O3), 316 stainless steel
- If it must be metal
- 316 stainless is attacked; Alloy 20 ratings are mixed and Hastelloy C is only good. Stay with plastics.
- Peristaltic tubing
- Avoid Flex-A-Prene and Flex-A-Thane. Flex-A-Chem is rated to 48 %; no tube rating above.
- PVDF preferred
- FKM, not EPDM
- Avoid 316
- Depends on strength
Why
HF calls for PVDF (Kynar) or PTFE wetted parts with FKM (Viton) seals, all rated excellent up to 70 %. Plain PP is also rated excellent to 70 %, but glass-filled PP is attacked, and PVC is only good. Ceramic check balls, EPDM and 316 stainless are rated not recommended. Above 70 % use PTFE seals.
From our applications engineers. Every pick is rated A or B by the guides at that strength.
13 of 13 materials
| Material | 0–40 % | 40–70 % | 70–100 % |
|---|---|---|---|
| elastomer Usual pick | |||
| plastic | |||
| plastic | |||
| plastic | |||
| plastic Usual pick | |||
| elastomer | |||
| plastic | – | ||
| metal | |||
| plastic | |||
| plastic | |||
| plastic Avoid | |||
| metal Avoid | |||
| elastomer Avoid |
- Excellent
- Good
- Fair
- Poor
- – No data
Bars: our confidence, 1 to 3. A temperature under the bars is the lowest limit a guide states. Orange dot: use with care; open the rating for why. Select any rating for the detail.
Ratings combine published chemical guides, weighted, with Cole-Parmer's printed chart breaking ties. Check the maker and your own conditions before you order. Dataset 2026-11-16-7f6e10a9