Hexane
Formula C6H14 · CAS 110-54-3
Used asTEAL (triethylaluminum)
What people pick
HeadPVDF (Kynar)
SealsFKM (Viton)
- Also works
- PVC (rigid), Polypropylene, PTFE (Teflon), Nitrile (Buna-N, NBR)
- Avoid
- EPDM, Aflas (TFE/P, FEPM)
- Peristaltic tubing
- Flex-A-Thane / PTB only: no pump tube is rated A; Flex-A-Thane rated good. Avoid Flex-A-Prene and Flex-A-Chem (rated D).
- PVDF preferred
- FKM, not EPDM
- Attacks plastics
Why
PVDF (Kynar) is the plastic head rated A. PVC and PP are B: PP slowly swells, fine cold but not for warm or continuous solvent duty. FKM (Viton) or nitrile seals rate A; EPDM fails.
From our applications engineers. Every pick is rated A or B by the guides at that strength.
13 of 13 materials
| Material | Strength not stated |
|---|---|
| metal | |
| elastomer Usual pick | |
| metal | |
| plastic | |
| plastic Usual pick | |
| plastic | |
| plastic | |
| plastic | |
| plastic | |
| plastic | |
| elastomer Avoid | |
| elastomer Avoid | |
| plastic |
- Excellent
- Good
- Fair
- Poor
- – No data
Bars: our confidence, 1 to 3. A temperature under the bars is the lowest limit a guide states. Orange dot: use with care; open the rating for why. Select any rating for the detail.
Ratings combine published chemical guides, weighted, with Cole-Parmer's printed chart breaking ties. Check the maker and your own conditions before you order. Dataset 2026-11-16-7f6e10a9