Formic Acid
Formula CH2O2 · CAS 64-18-6
Also called Aminic acid, Carbonous acid, Formylic acid, Hydrogen carboxylic acid, Hydroxy(oxo)methane, Metacarbonoic acid, Methanoic acid, Oxocarbinic acid, Oxomethanol
Sold at 85% · 94% · 99.7%
What people pick
- Also works
- PVDF (Kynar), PVC (rigid), Hypalon (CSPE / CSM)
- Avoid
- FKM (Viton), Aflas (TFE/P, FEPM), Nitrile (Buna-N, NBR)
- If it must be metal
- 316 stainless steel
- Peristaltic tubing
- Flex-A-Chem / CR, Santoprene (EPDM/PP TPV)Flex-A-Prene rated B (good). Avoid Flex-A-Thane (rated D).
- EPDM, not FKM
Why
Formic acid suits PP or PVDF (Kynar) heads, both rated excellent; PVC is only good. As with acetic acid, EPDM is the seal: FKM (Viton) is rated not recommended and TFE/P (AFLAS) fair to poor. 316 stainless is rated excellent.
From our applications engineers. Every pick is rated A or B by the guides at that strength.
13 of 13 materials
| Material | Strength not stated |
|---|---|
| metal | |
| plastic | |
| metal | |
| plastic Usual pick | |
| plastic | |
| plastic | |
| plastic | |
| elastomer Usual pick | |
| plastic | |
| plastic | |
| elastomer Avoid | |
| elastomer Avoid | |
| plastic |
- Excellent
- Good
- Fair
- Poor
- – No data
Bars: our confidence, 1 to 3. A temperature under the bars is the lowest limit a guide states. Orange dot: use with care; open the rating for why. Select any rating for the detail.
Ratings combine published chemical guides, weighted, with Cole-Parmer's printed chart breaking ties. Check the maker and your own conditions before you order. Dataset 2026-11-16-7f6e10a9