Ferric Chloride
Formula FeCl3 · CAS 7705-08-0
Also called Flores martis, Molysite
Sold at 40% FeCl3 (sold 37-42%) (usual)
What people pick
Any of these; no need to pick on compatibility.
- Also works
- CPVC, PTFE (Teflon)
- Avoid
- 316 stainless steel, Alloy 20 (Carpenter 20)
- If it must be metal
- No metal is rated A; Hastelloy C is rated B.
- Peristaltic tubing
- Flex-A-Prene / XL, Flex-A-Chem / CR, Flex-A-Thane / PT, Santoprene (EPDM/PP TPV), Versilon tubing (grade not stated)
- Most materials work
- Avoid 316
Why
Ferric chloride is pumped in PVC, PP or PVDF (Kynar) heads with FKM (Viton), EPDM or TFE/P (AFLAS) seals; all are rated A with high confidence. Keep stainless steel and Alloy 20 out of the wetted path: ferric chloride is the textbook chemical for pitting them. No metal is rated A; Hastelloy C is rated B.
From our applications engineers. Every pick is rated A or B by the guides at that strength.
13 of 13 materials
| Material | Strength not stated |
|---|---|
| plastic | |
| elastomer Usual pick | |
| plastic | |
| elastomer Usual pick | |
| elastomer Usual pick | |
| plastic | |
| plastic | |
| plastic Usual pick | |
| plastic | |
| plastic Usual pick | |
| plastic Usual pick | |
| metal | |
| metal Avoid |
What the guides note
“Iron Chloride (see ferric chloride)”
“Recommend liquid end flush”
- Excellent
- Good
- Fair
- Poor
- – No data
Bars: our confidence, 1 to 3. A temperature under the bars is the lowest limit a guide states. Orange dot: use with care; open the rating for why. Select any rating for the detail.
Ratings combine published chemical guides, weighted, with Cole-Parmer's printed chart breaking ties. Check the maker and your own conditions before you order. Dataset 2026-11-16-7f6e10a9