1,4-Dioxane

Formula C4H8O2 · CAS 123-91-1

Also called Diethylene ether, Dioxan, p-Dioxane

Pumping notes
Freezes near room temperature

What people pick

HeadPTFE (Teflon)
SealsFFKM or PTFE (Teflon)

EPDM is B, the best common elastomer.

Also works
EPDM
Avoid
PVC (rigid), Polypropylene, PVDF (Kynar), CPVC, FKM (Viton), Nitrile (Buna-N, NBR), Aflas (TFE/P, FEPM)
If it must be metal
316 stainless steel316 stainless rates A if a metal pump suits.
Peristaltic tubing
No pump tube suits it: Flex-A-Prene D, Flex-A-Chem D, Flex-A-Thane D.
  • PTFE only
  • Attacks plastics
  • Seal choice is critical
Why

Dioxane attacks PVC, PP and PVDF, so PTFE is the only plastic head rated A; 316 stainless also rates A. FFKM is the only elastomer rated A; EPDM is B and FKM (Viton) fails.

From our applications engineers. Every pick is rated A or B by the guides at that strength.

13 of 13 materials

MaterialStrength not stated
metal
plastic
Usual pick
metal
elastomer
plastic
plastic
plastic
Avoid
elastomer
Avoid
plastic
Avoid
elastomer
Avoid
plastic
Avoid
plastic
plastic
Avoid
  • Excellent
  • Good
  • Fair
  • Poor
  • – No data

Bars: our confidence, 1 to 3. A temperature under the bars is the lowest limit a guide states. Orange dot: use with care; open the rating for why. Select any rating for the detail.

Ratings combine published chemical guides, weighted, with Cole-Parmer's printed chart breaking ties. Check the maker and your own conditions before you order. Dataset 2026-11-16-7f6e10a9