Dimethyl Disulfide (DMDS)
Formula CH3SSCH3 · CAS 624-92-0
What people pick
FKM rating rests on one O-ring guide; a PTFE diaphragm adds margin.
- Also works
- FFKM, Nitrile (Buna-N, NBR)
- Avoid
- EPDM
- If it must be metal
- 316 stainless is likely (estimate only); no guide rates the metals for DMDS.
- Peristaltic tubing
- No maker tube rating.
- Few guides rate it
- FKM, not EPDM
- Attacks plastics
Why
No guide in our data rates a plastic head or a metal for DMDS; those ratings are estimates. The estimates point to PTFE and 316 stainless (likely), with PVC, CPVC and PP poor, and in practice DMDS injection is a stainless or PTFE job. For seals the guide data is clear: FKM (Viton) rates A and EPDM fails.
From our applications engineers. Every pick is rated A or B by the guides at that strength.
13 of 13 materials
| Material | Strength not stated |
|---|---|
| elastomer Usual pick | |
| plastic | |
| metal | |
| metal | |
| elastomer | |
| plastic | |
| plastic | |
| plastic | |
| plastic | |
| elastomer Avoid | |
| plastic | |
| plastic | |
| plastic |
- Excellent
- Good
- Fair
- Poor
- Estimate
- – No data
Bars: our confidence, 1 to 3. A temperature under the bars is the lowest limit a guide states. Orange dot: use with care; open the rating for why. Grey: an estimate, because no guide rates it. Select any rating for the detail.
Ratings combine published chemical guides, weighted, with Cole-Parmer's printed chart breaking ties. Check the maker and your own conditions before you order. Dataset 2026-11-16-7f6e10a9