Denatured Alcohol
What people pick
HeadPolypropylene or PVDF (Kynar)
SealsEPDM or Aflas (TFE/P, FEPM)
- Also works
- FKM (Viton), Nitrile (Buna-N, NBR)
- Peristaltic tubing
- No maker tube rating.
- A class, check the SDS
Why
PP and PVDF (Kynar) heads rate A; PVC is likely fine but only estimated. EPDM and TFE/P (AFLAS) seals rate A; FKM (Viton) is B. Denaturants vary, so check the SDS.
From our applications engineers. Every pick is rated A or B by the guides at that strength.
13 of 13 materials
| Material | Strength not stated |
|---|---|
| metal | |
| elastomer Usual pick | |
| plastic Usual pick | |
| plastic | |
| plastic Usual pick | |
| elastomer Usual pick | |
| metal | |
| plastic | |
| plastic | |
| plastic | |
| elastomer | |
| plastic | |
| plastic |
- Excellent
- Good
- Fair
- Poor
- Estimate
- – No data
Bars: our confidence, 1 to 3. A temperature under the bars is the lowest limit a guide states. Orange dot: use with care; open the rating for why. Grey: an estimate, because no guide rates it. Select any rating for the detail.
Ratings combine published chemical guides, weighted, with Cole-Parmer's printed chart breaking ties. Check the maker and your own conditions before you order. Dataset 2026-11-16-7f6e10a9