Chlorosulfonic Acid
Formula ClHSO3 · CAS 7790-94-5
Also called Chloridosulfonic acid, Chloridosulphonic acid, Chlorinesulfonic acid, Chlorinesulphonic acid, Chlorosulfuric acid, Chlorosulphonic acid, Sulfuric chlorohydrin
What people pick
- Avoid
- PVC (rigid), Polypropylene, PVDF (Kynar), CPVC, FKM (Viton), EPDM, Aflas (TFE/P, FEPM), Hypalon (CSPE / CSM), Nitrile (Buna-N, NBR), 316 stainless steel
- If it must be metal
- Hastelloy C / Alloy C (grade not stated)316 stainless is rated not recommended.
- Peristaltic tubing
- No pump tube suits it: Flex-A-Prene D, Flex-A-Chem D, Flex-A-Thane D.
- PTFE only
- Seal choice is critical
- Avoid 316
Why
Chlorosulfonic acid attacks nearly every plastic and elastomer: PVC, PP, PVDF (Kynar), FKM (Viton), EPDM and TFE/P (AFLAS) are rated poor or not recommended. PTFE wetted parts with PTFE or FFKM (Kalrez) seals are the answer, or Hastelloy C if a metal is needed.
From our applications engineers. Every pick is rated A or B by the guides at that strength.
13 of 13 materials
| Material | Strength not stated |
|---|---|
| metal | |
| plastic Usual pick | |
| plastic Avoid | |
| plastic Avoid | |
| elastomer Avoid | |
| elastomer Avoid | |
| plastic | |
| plastic Avoid | |
| metal Avoid | |
| plastic | |
| plastic | |
| plastic Avoid | |
| elastomer Avoid |
- Excellent
- Good
- Fair
- Poor
- – No data
Bars: our confidence, 1 to 3. A temperature under the bars is the lowest limit a guide states. Orange dot: use with care; open the rating for why. Select any rating for the detail.
Ratings combine published chemical guides, weighted, with Cole-Parmer's printed chart breaking ties. Check the maker and your own conditions before you order. Dataset 2026-11-16-7f6e10a9