Chlorinated Solvents (incl. Dry-Cleaning / Degreasing Fluids)
What people pick
Look up the specific solvent; methylene chloride is harder on both.
- Also works
- PTFE (Teflon)
- Avoid
- Polypropylene, EPDM, Nitrile (Buna-N, NBR), Aflas (TFE/P, FEPM)
- Peristaltic tubing
- No maker tube rating.
- A class, check the SDS
- Attacks plastics
- PVDF preferred
- FKM, not EPDM
Why
A class entry: check which solvent. Chlorinated solvents attack PVC, PP and CPVC, so the plastic head is PVDF (Kynar), and the seal is FKM (Viton); EPDM, nitrile and TFE/P (AFLAS) fail. Both PVDF and FKM drop to B with methylene chloride.
From our applications engineers. Every pick is rated A or B by the guides at that strength.
13 of 13 materials
| Material | Strength not stated |
|---|---|
| metal | |
| plastic | |
| elastomer Usual pick | |
| plastic Usual pick | |
| metal | |
| elastomer Avoid | |
| plastic Avoid | |
| elastomer Avoid | |
| plastic | |
| plastic | |
| plastic | |
| plastic | |
| plastic |
- Excellent
- Good
- Fair
- Poor
- Estimate
- – No data
Bars: our confidence, 1 to 3. A temperature under the bars is the lowest limit a guide states. Orange dot: use with care; open the rating for why. Grey: an estimate, because no guide rates it. Select any rating for the detail.
Ratings combine published chemical guides, weighted, with Cole-Parmer's printed chart breaking ties. Check the maker and your own conditions before you order. Dataset 2026-11-16-7f6e10a9