Chemical compatibility
Find a chemical, then compare the materials you care about.
Narrows the materials to the ones that brand offers
Compare materials (up to 8)
“Cooling tower chemical” usually means
- Sodium Hypochloriteusually 0–20 %our assumption
- Etidronic Acidour assumption
- Sulfuric Acidusually 95–100 %our assumption
- Sodium Bromideour assumption
Cooling programs: scale/corrosion inhibitor blend + oxidising/non-oxidising biocide + acid/pH.
4 chemicals
- Sodium Hypochlorite0–20 % · 20–100 %Usual pick: PVC head · FKM sealsPVC is the usual headOff-gassesAvoid 316
- PVC (rigid)
- PVDF (Kynar)
- PTFE (Teflon)
- 316 stainless steel
- EPDM
- Etidronic AcidAll strengthsUsual pick: PVDF or Glass-filled polypropylene head · FKM or EPDM or Aflas sealsFew guides rate it
- PVC (rigid)
- PVDF (Kynar)
- PTFE (Teflon)
- 316 stainless steel
- EPDM
- Sulfuric Acid0–10 % · 10–75 % · 75–95 % · 95–100 %Usual pick: PVDF head · FKM sealsPVDF preferredFKM, not EPDMDepends on strength
- PVC (rigid)
- PVDF (Kynar)
- PTFE (Teflon)
- 316 stainless steel
- EPDM
- Sodium BromideAll strengthsUsual pick: PVC or Polypropylene or PVDF head · FKM or EPDM sealsMost materials workAvoid 316
- PVC (rigid)
- PVDF (Kynar)
- PTFE (Teflon)
- 316 stainless steel
- EPDM
Squares run from the lowest strength to the highest. Open a chemical for every material and what each guide says.